Recent progress in photoinitiated ring-opening metathesis polymerization (photoROMP) has enabled the lithographic production of patterned films from olefinic resins. Recently, we reported the use of a latent ruthenium catalyst (HeatMet) in combination with a photosensitizer (2-isopropylthioxanthone) to rapidly photopolymerize dicyclopentadiene (DCPD) formulations upon irradiation with UV light. While this prior work was limited in terms of catalyst and photosensitizer scope, a variety of alternative catalysts and photosensitizers are commercially available that could allow for tuning of thermomechanical properties, potlifes, activation rates, and irradiation wavelengths. Herein, 14 catalysts and 8 photosensitizers are surveyed for the photoROMP of DCPD and the structure–activity relationships of the catalysts examined. Properties relevant to stereolithography additive manufacturing (SLA AM)-potlife, irradiation dose required to gel, conversion-are characterized to develop catalyst and photosensitizer libraries to inform development of SLA AM resin systems. Two optimized catalyst/photosensitizer systems are demonstrated in the rapid SLA printing of complex, multidimensional pDCPD structures with microscale features under ambient conditions.
Solid state nuclear magnetic resonance (NMR) spectroscopy and small-to wide-angle X-ray scattering (SWAXS) methods were used to characterize the heterogeneous dynamics and polymer domain structure in rubber modified thermoset materials containing the diglycidyl ether of bisphenol A (DGEBA) epoxy resin and a mixture of Jeffamine reactive rubber and 4,4-diaminodicyclohexylmethane (PACM) amine curing agent. The polymer chain dynamics and morphologies as a function of the PACM/Jeffamine ratio were determined. Using dipolar-filtered NMR experiments, the resulting networks are shown to be composed of mobile and rigid regions that are separated on nanometer length scales, along with a dynamically immobilized interface region. Proton NMR spin diffusion experiments measured the dimensions of the mobile phase to range between 9 and 66 nm and varied with the relative PACM concentration. Solid state 13C magic angle spinning NMR experiments show that the highly mobile phase is composed entirely of the dynamically flexible polyether chains of the Jeffamine rubber, the immobilized interface region is a mixture of DGEBA, PACM, and the Jeffamine rubber, with the PACM cross-linked to DGEBA predominantly residing in the rigid phase. The SWAXS results showed compositional nanophase separation spanning the 11–77 nm range. These measurements of the nanoscale compositional and dynamic heterogeneity provide molecular level insight into the very broad and controllable glass transition temperature distributions observed for these highly cross-linked polymer networks.
Once limited to chain-growth polymerizations, fine control over polymerization-induced phase separation (PIPS) has recently been demonstrated in rubber-toughened thermoset materials formed through step-growth polymerizations. The domain length scales of these thermoset materials can be elegantly tuned by utilizing a binary mixture of curing agents (CAs) that individually yield disparate morphologies. Importantly, varying the composition of the binary mixture affects characteristics of the materials such as glass transition temperature and tensile behavior. Here, we establish a full phase diagram of PIPS in a rubber-toughened epoxy system tuned by a binary CA mixture to provide a robust framework of phase behaviour. X-Ray scattering in situ and post-PIPS is employed to elucidate the PIPS mechanism whereby an initial polymerization-induced compositional fluctuation causes nanoscale phase separation of rubber and epoxy components prior to local chain crosslinking and potential macrophase separation. We further demonstrate the universality of this approach by alternatively employing binary epoxy or binary rubber mixtures to achieve broad variations in morphology and glass transitions.
The development of chemistry is reported to implement selective dual-wavelength olefin metathesis polymerization for continuous additive manufacturing (AM). A resin formulation based on dicyclopentadiene is produced using a latent olefin metathesis catalyst, various photosensitizers (PSs) and photobase generators (PBGs) to achieve efficient initiation at one wavelength (e.g., blue light) and fast catalyst decomposition and polymerization deactivation at a second (e.g., UV-light). This process enables 2D stereolithographic (SLA) printing, either using photomasks or patterned, collimated light. Importantly, the same process is readily adapted for 3D continuous AM, with printing rates of 36 mm h–1 for patterned light and up to 180 mm h–1 using un-patterned, high intensity light.
Polymerization-induced phase separation enables fine control over thermoset network morphologies, yielding heterogeneous structures with domain sizes tunable over 1-100 nm. However, the controlled chain-growth polymerization techniques exclusively employed to regulate the morphology at these length scales are unsuitable for a majority of thermoset materials typically formed through step-growth mechanisms. By varying the composition of a binary curing agent mixture in a classic rubber-toughened epoxy thermoset, where the two curing agents are selected based on disparate compatibility with the rubber, we demonstrate facile tunability over morphology through a single compositional parameter. Indeed, this method yields morphologies spanning the nano-scale to the macro-scale, controlled by the relative reactivities and thermodynamic compatibility of the network components. We further demonstrate a profound connection between chain dynamics and microstructure in these materials, with the tunable morphology enabling exquisite variations in glass transition. In addition, previously unattainable control over tensile mechanical properties is realized, including atypical increase of elongation at failure while maintaining the modulus and ultimate strength.