Cured Properties
Curing Properties
Cured Properties
- 100 pbw adduct of digylcidyl ether of bisphenol A (Epon 828) and Hycar 1300×8 carboxyl terminated butadiene acrylonitrile rubber (CTBN)
- 12 pbw diethanolamine
- 28 pbw 3M D32 glass microballoons
- Cured 24 hours at 71C