Cured Properties
Composition:
- 100 pbw Sylgard 184 base resin from Dow Corning
- 10 pbw Sylgard 184 curing agent from Dow Corning
- 78, 125, or 190 pbw (25, 35, or 45vol%) Teco-Sil 44CSS silica
- cured 24 hours at room temp and 2 hrs at 71C
Cured Properties
Composition: