Reference:
Adolf, D. B.; et al
Polymer; 2010; 51: 1530-1539.
In two tests, a “2N history” was applied to the annealed fiber by heating to 200C under no load, applying 2N, cooling to 0C under 2N, and releasing the load at 0C. Two “isoforce tests” under constant loads of 0 or 8N were then begun.
DOWNLOAD DATA FILES
Annealed Fiber Under No Load | Fiber with 2N History Under No Load | Fiber with 2N History under an 8N Load |
---|---|---|
Temp (C) | Temp (C) | Temp (C) |
% Linear Strain | % Linear Strain | % Linear Strain |