Nylon

The DuPont Nylon monofilament fibers (0.32 mm diameter) have considerable residual stress from processing. Fibers were therefore annealed prior to testing by heating to 200C under no load and cooling to the test temperature again under no load.

Reference:

Adolf, D. B.; et al